J556FeXG Pipe Welding Electrode
AWS:E8018-G
Current:Suitable for filling welding and cosmetic welding on medium-carbon steel and low-alloy steel pipes with corresponding strength grades, and also used for downward fillet welding and downward butt groove welding on structural steel with the same strength gr
J556FeXG |
According with GB E5518-G Corresponding with AWS E8018-G |
||||||||||||
|
|||||||||||||
|
|||||||||||||
Chemical Composition of Deposited Metal (%)
|
|||||||||||||
Mechanical Properties of Deposited Metal
|
|||||||||||||
Diffusible Hydrogen Content in Deposited Metal: ≤6.0ml/100g(Glycerine Hydrogen Test) |
|||||||||||||
X-ray Radiographic Inspection: ⅠDegree |
|||||||||||||
Reference Current (AC, DC+)
|
|||||||||||||
Instructions: 1.The electrodes must be baked under 350-400℃ for an hour before welding, and used as soon as baking is completed. 2.The stains on the weldments, such as rust, oil stains, moisture, etc., must be cleared away before welding. 3.When welding, short arc must be used, and it is suitable to manipulate the electrodes directly downwards or with a little downward crescent weaving. |
|