Cr9MoVNi stanless steel welding rod

item model trade mark coating type current type
WSR717 Cr9MoVNi —— Low hydrogen type sodium DC+
standard Applicable standards/model
Q/SS.J13-2006 R717 AWS A5.5 E9015-B9
Deposited metal chemical composition
C Mn Si S P Cr Ni Mo Cu other
≤0.12
0.04
0.60-1.20
0.62
≤0.50
0.21
≤0.030
0.008
≤0.035
0.020
8.0-10.0
9.9
0.40-1.00
0.80
0.80-1.10
0.95
_ V:0.15-0.40 (0.18)
Nb:0.02-0.08 (0.04)
preperity uesage
tensile strength yeild srength elongation
≥590
730-830
_ ≥15
17-20
_ tem at 600℃ with Cr9Mo1、9MoNiV heat-reasistant steel