R802 heat-resistant steel electrode
R802
GB:E11MoVNi-16
AWS:
Current:Used for welding Cr11MoV heat-resistant steel structures below 565��.
Main Applications:
AWS:
Current:Used for welding Cr11MoV heat-resistant steel structures below 565��.
Main Applications:
R802 |
According with GB E11MoVNi-16 |
||||||||||||||||||||
|
|||||||||||||||||||||
|
|||||||||||||||||||||
Chemical Composition of Deposited Metal (%)
|
|||||||||||||||||||||
Mechanical Properties of Deposited Metal
|
|||||||||||||||||||||
Reference Current (AC, DC)
|
|||||||||||||||||||||
Instructions: 1.The electrodes must be baked under about 350℃ for an hour before welding, and used as soon as baking is completed. 2. The weldments should be preheated to 350-400℃ before welding. 3.The stains on the weldments, such as rust, oil stains, moisture, etc., must be cleared away before welding. |
|