Acrylic Acid Modified Chlorinated Polyvinyl Chloride Anticorrosive Finish
Acrylic Acid Modified Chlorinated Polyvinyl Chloride Anticorrosive Finish (Different Colors) (Use for steel structure)
Characteristics:paint film dry quickly, excellent resistance of
corrosion and moist property, good chemicla resistance property, resistance of
spread burning, it can be stilled constructed in -20℃
Uses:applicable for chemical
machinery、equipment、pipeline
etc. metal, anticorrosive coating of cement part, anticorrosion of acid、 alkali and chemical medicine.
Technical target:
Mixing ratio: single
component
Standard film thickness: Dry: 30μm/coat
Academic spreading rate: 0.11kg/ m2/30μm
Solid contents: 40%
Humidity requirement: below 85%
Drying time & Coating interval
Temperature(℃) |
0 |
10 |
20 |
30 |
Dry to touch(hrs) |
30 |
20 |
15 |
10 |
Dry semi-hard(hrs) |
4 |
3 |
1.5 |
1 |
Min. interval(hrs) |
10 |
9 |
7 |
5 |
Substrate
treatment:Primers(intermediate paint)surface should be clean and dry, no feculence.
Sweep remove dust etc. feculence by pressure-air. If construction environment
humidity >70%, add measured FX-2 chlorinated polyvinyl chloride
damp-proofing admixture.
Matching:Applicable substrate:Substrate which sprayed chlorinated
polyvinyl chloride primer
CONTACT WITH US NOW